Use of electrochemical noise to detect stress corrosion crack initiation in simulated BWR environments

โœ Scribed by J. Hickling; D. F. Taylor; P. L. Andresen


Publisher
John Wiley and Sons
Year
1998
Tongue
German
Weight
299 KB
Volume
49
Category
Article
ISSN
0947-5117