UHV-compatible spectroscopic scanning Kelvin probe for surface analysis

✍ Scribed by I. Baikie; U. Petermann; B. Lägel


Book ID
117219228
Publisher
Elsevier Science
Year
1999
Tongue
English
Weight
145 KB
Volume
433-435
Category
Article
ISSN
0039-6028