Dense AI203 particle-Y-TZP matrix (AI203 < 40 vol %) composite was prepared by pressureless sintering at 1550~ Composites with 10-30 vol % AI=O 3 particles showed enhanced fracture toughness, bending strength and Vicker's hardness as compared to singlephase Y-TZP. The highest strength (1150 MPa) and
Toughening mechanisms and properties of mullite matrix composites reinforced by the addition of SiC particles and Y-TZP
β Scribed by J. S. Hong; X. X. Huang; J. K. Guo
- Publisher
- Springer
- Year
- 1996
- Tongue
- English
- Weight
- 894 KB
- Volume
- 31
- Category
- Article
- ISSN
- 0022-2461
No coin nor oath required. For personal study only.
π SIMILAR VOLUMES
AI203-SiC-ZrO 2 composites were investigated to obtain a better understanding of the effect of SiC particles and the stress-induced transformation of Y-TZP on its mechanical properties. The AI203-SiC-ZrO 2 composites were fabricated by hot pressing using y-AI203, SiC and Zr02 mixtures. Fracture toug
The wear behaviour of SiCp-reinforced aluminium composite produced by the molten metal mixing method was investigated by means of a pin-on-disc type wear rig. Abrasive wear tests were carried out on 5 vol.% SiCp and its matrix alloy against SiC and Al O emery papers on a steel counterface at a fixed