๐”– Bobbio Scriptorium
โœฆ   LIBER   โœฆ

Topmost surface analysis of an MgO-dissolved LiNbO3 single crystal with coaxial impact collision ion scattering spectroscopy

โœ Scribed by Kenji Tabata; Tetsuo Choso; Yousuke Nagasawa


Book ID
117219652
Publisher
Elsevier Science
Year
1999
Tongue
English
Weight
159 KB
Volume
433-435
Category
Article
ISSN
0039-6028