𝔖 Bobbio Scriptorium
✦   LIBER   ✦

Time-dependent characteristics of incipient plasticity in nanoindentation of a Ni3Al single crystal

✍ Scribed by Y.L Chiu; A.H.W Ngan


Book ID
108491850
Publisher
Elsevier Science
Year
2002
Tongue
English
Weight
404 KB
Volume
50
Category
Article
ISSN
1359-6454

No coin nor oath required. For personal study only.


πŸ“œ SIMILAR VOLUMES