Thermal conductivity of nitrous oxide is measured by the conductivity column method in the temperature range 50° to 900°C.\_The presently obtained experimental data suggest that it is necessary to take into account the relaxation of translational-internal energy exchange for nitrous oxide in the tem
Thermal oxidation of polypropylene in the temperature range of 120–280°c
✍ Scribed by Ariel Hoff; Sven Jacobsson
- Publisher
- John Wiley and Sons
- Year
- 1984
- Tongue
- English
- Weight
- 777 KB
- Volume
- 29
- Category
- Article
- ISSN
- 0021-8995
No coin nor oath required. For personal study only.
📜 SIMILAR VOLUMES
Although several authors have found anisotropy of the chemical reactivity of pyrolytic graphite they disagree regarding the existence of a temperature coefficient. New data are presented which together with earlier data show the rate ratio for the two major directions is temperature dependent with a
The oxidation of cobalt has been studied in CO-CO, mixtures in the temperature range 920°C-1200°C. The kinetics of oxidation were determined by using an aut.omatic recording vacuum balance. The mechanism of oxidation was studied through the analysis of kinetics and by marker studies, X-ray analysis
The ultimate properties of thermally oxidized polypropylene (PP) films have been determined. Attention was focused on the variation of draw stress, tensile strength, draw ratio, breaking extension, breaking factor, work of draw, and work of rupture, with a change in temperature and time of heat trea