The products obtained on vacuum pyrolysis of poly(p-N,N-diethylaminostyrene) are described. The effect of sample molecular weight and pyrolysis temperature are compared with that observed for polystyrene degraded under identical conditions. The liquid products were separated using gas-liquid chromat
โฆ LIBER โฆ
Thermal degradation of polymers. Part III. Vacuum pyrolysis of poly(m-aminostyrene); the products volatile at pyrolysis temperature which are liquid or gaseous at room temperature
โ Scribed by R. H. Still; P. B. Jones
- Publisher
- John Wiley and Sons
- Year
- 1969
- Tongue
- English
- Weight
- 438 KB
- Volume
- 13
- Category
- Article
- ISSN
- 0021-8995
No coin nor oath required. For personal study only.
๐ SIMILAR VOLUMES
Thermal degradation of polymers. XXIII.
โ
T. S. Ellis; R. H. Still
๐
Article
๐
1979
๐
John Wiley and Sons
๐
English
โ 465 KB
Thermal degradation of polymers. XXIV. V
โ
T. S. Ellis; R. H. Still
๐
Article
๐
1979
๐
John Wiley and Sons
๐
English
โ 498 KB
Comparative studies were made of the residue and the fraction volatile a t pyrolysis temperature, involatile a t ambient temperature obtained from polystyrene and poly(p-N,N-diethylaminostyrene) degraded under identical conditions. Poly(p-N,N-diethylaminostyrene) yielded a crosslinked glassy residue