Thermal degradation of aramids: Part I—Pyrolysis/gas chromatography/mass spectrometry of poly(1,3-phenylene isophthalamide) and poly(1,4-phenylene terephthalamide)

✍ Scribed by James R. Brown; Alan J. Power


Publisher
Elsevier Science
Year
1982
Tongue
English
Weight
616 KB
Volume
4
Category
Article
ISSN
0141-3910

No coin nor oath required. For personal study only.


📜 SIMILAR VOLUMES


Primary thermal degradation processes of
✍ Giorgio Montaudo; Concetto Puglisi; R. Rapisardi; Filippo Samperi 📂 Article 📅 1994 🏛 John Wiley and Sons 🌐 English ⚖ 590 KB

## Abstract The thermal degradation processes which occur in poly(ether‐sulfone) (PES) and poly(phenylene oxide) (PPO) have been studied by Direct Pyrolysis‐Mass Spectrometry (DPMS). The pyrolysis mass spectra of PES and PPO contain molecular ions up to __m/z__ 700, corresponding to pyrolysis compo

A study of thermal degradation of poly(a
✍ C. J. Tsai; L. H. Perng; Y. C. Ling 📂 Article 📅 1997 🏛 John Wiley and Sons 🌐 English ⚖ 205 KB 👁 2 views

Thermal degradation of poly(aryl-ether-ether-ketone) (PEEK) was investigated using stepwise pyrolysis/gas chromatography/mass spectrometry (Py/GC/MS) by consecutively heating the sample at fixed temperature intervals to achieve narrow temperature pyrolysis conditions. The individual mass chromatogra