Thermal degradation kinetics and mechanism of epoxidized natural rubber
โ Scribed by He, Canzhong (author);Wang, Yueqiang (author);Luo, Yongyue (author);Kong, Lingxue (author);Peng, Zheng (author)
- Book ID
- 120964538
- Publisher
- Walter de Gruyter GmbH & Co. KG
- Year
- 2013
- Tongue
- English
- Weight
- 382 KB
- Volume
- 33
- Category
- Article
- ISSN
- 0334-6447
No coin nor oath required. For personal study only.
๐ SIMILAR VOLUMES
The thermal degradation and thermooxidative degradation of epoxidized natural rubber (ENR) were studied by thermogravimetry (TG). In the thermal degradation of ENR, the initial temperature of weight loss T 0 ร 1.20B / 348, the temperature of maximum weight loss rate T p ร 1.07B / 392, and the final
## Abstract Oxidative degradation of epoxidized natural rubber (ENR) was effectively performed in latex phase by using periodic acid at 30ยฐC. The ENR was prepared from the epoxidation of natural rubber in latex phase using performic acid generated __in situ__ by the reaction of hydrogen peroxide an
Two sets (A and B) of bisphenol Aยฑdiglycidyl ether (DGEBA) based epoxy resin formulations were modiยฎed with epoxidized natural rubber (ENR 50) and its liquid version (LENR 50), and cured with amino propoxylate initiator/accelerator at ambient temperatures. The ENR 50 loading range was 1.6ยฑ5.9 wt%. B