The use of differential scanning calorimetry to study the reprocessing of poly(vinyl chloride)

โœ Scribed by J.A. Covas


Book ID
107846805
Publisher
Elsevier Science
Year
1993
Tongue
English
Weight
438 KB
Volume
34
Category
Article
ISSN
0032-3861

No coin nor oath required. For personal study only.


๐Ÿ“œ SIMILAR VOLUMES


Compatibility of poly(ethylene oxide)/po
โœ Issa A. Katime; M.S. Anasagasti; M.C. Peleteiro; R. Valenciano ๐Ÿ“‚ Article ๐Ÿ“… 1987 ๐Ÿ› Elsevier Science ๐ŸŒ English โš– 274 KB

This article refers to a study of the thermal behaviour of poly(ethylene oxide) and poly(vinyl chloride) blends in the solid state. The compatibility has been examined by differential scanning calorimetry. The influence of molecular masses of the polymers on their compatibility has been shown. The e