The surface analysis of a plasma modified contact lens surface by SSIMS
β Scribed by D. W. Fakes; M. C. Davies; A. Brown; J. M. Newton
- Publisher
- John Wiley and Sons
- Year
- 1988
- Tongue
- English
- Weight
- 378 KB
- Volume
- 13
- Category
- Article
- ISSN
- 0142-2421
No coin nor oath required. For personal study only.
π SIMILAR VOLUMES
Lithium niobate (LiNbO 3 ) is a widely used ferroelectric material with high electro-optic, non-linear optic, birefringent and photorefractive activities. Modification of the surface of LiNbO 3 single crystals is essential for its application in optoelectronics. We accomplished the surface modificat
## Abstract Of the several techniques available for surface modification, plasma processing has proved to be very appropriate. The low temperature plasma is a soft radiation source and it affects the material only over a few hundred angstroms deep, the bulk properties remaining unaffected. Plasma s
The modification of the PET fiber surface to render a higher degree of hydrophobicity by graft fluorination involves a surface layer of only a few nanometers thickness. The relatively low fraction of the modified surface layer presents difficulties in surface analysis. However, surface free energy c