𝔖 Bobbio Scriptorium
✦   LIBER   ✦

The relation between corrosion fatigue and stress corrosion cracking in AlZnMG alloys

✍ Scribed by T. Magnin; P. Rieux


Book ID
116062520
Publisher
Elsevier Science
Year
1987
Weight
318 KB
Volume
21
Category
Article
ISSN
0036-9748

No coin nor oath required. For personal study only.