The production of acoustic contact in the study of polymers in the temperture range 2.1 to 240 K
β Scribed by I.I. Perepechko; P.D. Golub'
- Book ID
- 103051529
- Publisher
- Elsevier Science
- Year
- 1973
- Tongue
- English
- Weight
- 188 KB
- Volume
- 13
- Category
- Article
- ISSN
- 0011-2275
No coin nor oath required. For personal study only.
β¦ Synopsis
in the volt-watt sensitivity is shifted in the direction of smaller bolometer resistances. If the maximum sensitivity was observed for a resistance of 2 g2 in the isothermal regime, then it was at 1 ~2 in the non-isothermal regime. The observed shift in the sensivity maximum agrees with the data reported earlier. 7