THE PREPARATION OF BORIC ACID ANHYDRIDE AND ITS EFFICIENCY AS A DRYING AGENT

โœ Scribed by Walton, James H.; Rosenbaum, Chester K.


Book ID
127323920
Publisher
American Chemical Society
Year
1928
Tongue
English
Weight
211 KB
Volume
50
Category
Article
ISSN
0002-7863

No coin nor oath required. For personal study only.


๐Ÿ“œ SIMILAR VOLUMES


The elastic property of polyvinyl alcoho
โœ Huei-Hsiung Wang; Tien-Wei Shyr; Mei-Shan Hu ๐Ÿ“‚ Article ๐Ÿ“… 1999 ๐Ÿ› John Wiley and Sons ๐ŸŒ English โš– 172 KB ๐Ÿ‘ 2 views

The elastomers of polyvinyl alcohol gel were made from the polyvinyl alcohol polymer, with boric acid added as a crosslinking agent, in the mixed solvent of dimethyl sulfoxide and water. From the experimental results, the viscosity of polyvinyl alcohol solution is found to increase not only with an

Amic acids of alphamethyl styrene and ma
โœ M. A. Shenoy; Kusum S. Joshi ๐Ÿ“‚ Article ๐Ÿ“… 2000 ๐Ÿ› John Wiley and Sons ๐ŸŒ English โš– 122 KB ๐Ÿ‘ 1 views

Alphamethyl styrene (AMS) and maleic anhydride (MAn) were copolymerized in 2-butanone using benzoyl peroxide as initiator. Low molecular weight (8000) of alphamethyl styrene-maleic anhydride copolymer was prepared using AMS dimer as a chain-transfer agent. This copolymer was then treated with two di