The pitting corrosion of pure and low alloyed copper in chloride-containing borate buffered solutions
β Scribed by W. Qafsaoui; G. Mankowski; F. Dabosi
- Book ID
- 115847615
- Publisher
- Elsevier Science
- Year
- 1993
- Tongue
- English
- Weight
- 399 KB
- Volume
- 34
- Category
- Article
- ISSN
- 0010-938X
No coin nor oath required. For personal study only.
π SIMILAR VOLUMES
The pitting corrosion of 316 stainless steel (SS) in phosphate-borate buffer (pH 8 .00) containing 0.5 M NaCl at 25'C is studied through current transients run under a constant potential step, potentiodynamic runs and scanning electron microscopy . According to the potential and time windows differe
The influence of the passive layer properties on the pitting corrosion of 316SS was studied in phosphate-borate buffer containing chloride ions by using potential step and potentiodynamic techniques complemented with scanning electron microscopy. The increase of the anodization time in the passive r