The pitting corrosion behavior of shear bands in a Zr-based bulk metallic glass

✍ Scribed by X.P. Nie; Q.P. Cao; Z.F. Wu; Y. Ma; X.D. Wang; S.Q. Ding; J.Z. Jiang