๐”– Bobbio Scriptorium
โœฆ   LIBER   โœฆ

The nucleation of grain boundary voids in a nickel-base superalloy during high temperature creep

โœ Scribed by K. Shiozawa; J.R. Weertman


Book ID
116060998
Publisher
Elsevier Science
Year
1982
Weight
311 KB
Volume
16
Category
Article
ISSN
0036-9748

No coin nor oath required. For personal study only.


๐Ÿ“œ SIMILAR VOLUMES