The microstructure and thermoelectric properties of rapid solidified p-type Sb2Te3–25wt.%Bi2Te3 alloys

✍ Scribed by Moon, ChulDong; Kim, Taek-Soo


Book ID
118042300
Publisher
Elsevier Science
Year
2012
Tongue
English
Weight
1010 KB
Volume
536
Category
Article
ISSN
0925-8388

No coin nor oath required. For personal study only.


📜 SIMILAR VOLUMES


Thermoelectric properties of fine-graine
✍ A. A. Joraide 📂 Article 📅 1995 🏛 Springer 🌐 English ⚖ 389 KB

P-type semiconductor alloy compacts of the composition (Bi2Te3)25 -(Sb2Te3)75 with grain size (L) in the range 30 > L > 20 lam, 20 > L > 151am, 15 > L > 10 lam, 10 > L > 5 and L < 5 ~tm were prepared by cold press at a pressure of 77 • 107 Nm -2. The samples were sintered at 673 K. Measurements of t