𝔖 Bobbio Scriptorium
✦   LIBER   ✦

The low cycle fatigue deformation response of a single-crystal superalloy at 650°C: Gabb, T.P., Welsch, G., Miner, R.V. and Gayda, J. Mater. Sci. Eng. Feb. 1989 A A108, (1–2), 189–202


Publisher
Elsevier Science
Year
1989
Tongue
English
Weight
125 KB
Volume
11
Category
Article
ISSN
0142-1123

No coin nor oath required. For personal study only.