The kinetics describing the thermal decomposition of Li 4 SiO 4 and Li 2 SiO 3 have been analysed. While Li 4 SiO 4 decomposed on Li 2 SiO 3 by lithium sublimation, Li 2 SiO 3 was highly stable at the temperatures studied. Li 4 SiO 4 began to decompose between 900 and 1000 1C. However, at 1100 1C or
The kinetic behaviour and thermal stability of commercially available explosives
✍ Scribed by E. L. M. Krabbendam-LaHaye; W. P. C. de Klerk; R. E. Krämer
- Publisher
- Springer Netherlands
- Year
- 2005
- Tongue
- English
- Weight
- 405 KB
- Volume
- 80
- Category
- Article
- ISSN
- 0022-5215
No coin nor oath required. For personal study only.
📜 SIMILAR VOLUMES
The inýuence of Korver's de-ashing procedure on the changes in the thermal stability and porosity of three commercial granular activated carbons : D43/1 (Carbo-Tech, Essen, Germany), AHD, and WD-extra (Hajno wka, Poland) was investigated. For original carbons, carbons treated only with concentrated
Columnar discotic materials are considered for applications in the area of photoconductivity and light-emitting diodes. A major requirement is their stability at elevated temperatures and in the presence of oxygen. The thermal and thermo-oxidative behaviour of discotic triphenylene derivatives was i