The fracture resistance of a Sic whisker/AlzO, matrix composite for the test temperature range of 20" to 1400ยฐC was determined using chevron-notched and straightnotched, three-point bend specimens. Crack mouth opening displacement (CMOD) was continuously monitored throughout the fracture tests, usin
โฆ LIBER โฆ
The interactions of an Al2O3-SiC-whisker-reinforced composite ceramic with liquid metals
โ Scribed by R. Barrett; T.F. Page
- Publisher
- Elsevier Science
- Year
- 1990
- Tongue
- English
- Weight
- 946 KB
- Volume
- 138
- Category
- Article
- ISSN
- 0043-1648
No coin nor oath required. For personal study only.
๐ SIMILAR VOLUMES
Elevated temperature fracture resistance
โ
M.G. Jenkins; A.S. Kobayashi; K.W. White; R.C. Bradt
๐
Article
๐
1988
๐
Elsevier Science
๐
English
โ 919 KB
The wear properties of an SiC-whisker-re
โ
L. Cao; Y. Wang; C.K. Yao
๐
Article
๐
1990
๐
Elsevier Science
๐
English
โ 400 KB
95/04019 Comparison of the dynamic fatig
๐
Article
๐
1995
๐
Elsevier Science
โ 187 KB
Oxidation kinetics of metallic inclusion
โ
N. A. Mariano; M. A. G. Tommaselli; S. E. Kuri
๐
Article
๐
2005
๐
John Wiley and Sons
๐
English
โ 235 KB
Many studies have been conducted to obtain toughness in ceramic-ceramic and metal-ceramic composites, using new processing techniques or by addition of metallic inclusions in the ceramic matrix. The oxidation behavior of metallic inclusions, niobium and nickel metallic particles embedded in an Al 2