The influence of temperature on the galvanic corrosion of a cast iron-stainless steel couple (prediction by boundary element method)

โœ Scribed by F.E. Varela; Y. Kurata; N. Sanada


Book ID
117087311
Publisher
Elsevier Science
Year
1997
Tongue
English
Weight
931 KB
Volume
39
Category
Article
ISSN
0010-938X

No coin nor oath required. For personal study only.


๐Ÿ“œ SIMILAR VOLUMES


Boundary element method predictions of t
โœ J. X. Jia; G. Song; A. Atrens ๐Ÿ“‚ Article ๐Ÿ“… 2005 ๐Ÿ› John Wiley and Sons ๐ŸŒ German โš– 582 KB

This research investigated the galvanic corrosion of the magnesium alloy AZ91D coupled to steel. The galvanic current distribution was measured in 5% NaCl solution, corrosive water and an auto coolant. The experimental measurements were compared with predictions from a Boundary Element Method (BEM)