Controlling the formation of wrinkles in
โ
Wen Hui Duan; Kai Gong; Quan Wang
๐
Article
๐
2011
๐
Elsevier Science
๐
English
โ 750 KB
The initiation and development of wrinkles in a single layer graphene sheet subjected to inplane shear displacements are investigated. The dependence of the wavelength and amplitude of wrinkles on the applied shear displacements is explicitly obtained with molecular mechanics simulations. A continuu