The formation of cuprous oxide films on α-brass stress-corrosion fracture surfaces

✍ Scribed by R.P.M. Procter; G.N. Stevens


Book ID
115845885
Publisher
Elsevier Science
Year
1975
Tongue
English
Weight
603 KB
Volume
15
Category
Article
ISSN
0010-938X

No coin nor oath required. For personal study only.