Nickel aluminide-alumina nanocomposite was prepared by a conventional powder metallurgy technique. Nanosize alumina as dispersed phase was mixed with Ni and Al powder in a planetary ball mill for 4 h at 175 rpm. The mixture was then compacted using a hydraulic press at 400 MPa for 15 min. Sintering