## Abstract Fretting wear is often found at the contact surfaces of a tight assembly where smallβamplitude oscillatory movement occurs, which can be the concealed origin of some enormous accidents. Employment of solid lubrication coatings, as one of effective measurements to palliate the fretting d
β¦ LIBER β¦
The effects of hertzian stress and test atmosphere on the friction coefficients of MoS2 coatings
β Scribed by L.E. Pope; J.K.G. Panitz
- Publisher
- Elsevier Science
- Year
- 1988
- Tongue
- English
- Weight
- 822 KB
- Volume
- 36
- Category
- Article
- ISSN
- 0257-8972
No coin nor oath required. For personal study only.
π SIMILAR VOLUMES
Effect of contact configuration on the d
β
D. B. Luo; V. Fridrici; Ph. Kapsa; T. Murakami
π
Article
π
2009
π
John Wiley and Sons
π
English
β 933 KB
The effect of lubricant additives on the
β
J. Kosanov; J.G. Lenard; J. Uhrig; B. Wallfarth
π
Article
π
2006
π
Elsevier Science
π
English
β 679 KB
Effects of temperature and ion-to-atom r
β
L.E. Seitzman; R.N. Bolster; I.L. Singer
π
Article
π
1995
π
Elsevier Science
π
English
β 540 KB
Effect of additive interactions on the f
β
Wei Jianjun; Xue Qunji
π
Article
π
1992
π
Elsevier Science
π
English
β 652 KB
Effect of substrate material and residua
β
Siegfried Hofmann; Hermann A. Jehn
π
Article
π
1990
π
Elsevier Science
π
English
β 734 KB
The effects of processing variables on s
β
Jason A. Payne; Lorraine F. Francis; Alon V. McCormick
π
Article
π
1997
π
John Wiley and Sons
π
English
β 359 KB
π 2 views
A cantilever deflection technique was used to monitor stress development during ultraviolet photo-cure of acrylate coatings to the glassy state. Two coating systems were studied: a trifunctional monomer (trimethylol propane triacrylate, TMPTA) and a tetrafunctional monomer (pentaerythritol tetraacry