𝔖 Bobbio Scriptorium
✦   LIBER   ✦

The Effect of Gold Pre-Deposition on the Oxidation Behavior of CPTi and Ti6Al4V Alloy

✍ Scribed by Z. X. Zhang; H. Dong; T. Bell; B. S. Xu


Publisher
Springer-Verlag
Year
2006
Tongue
English
Weight
758 KB
Volume
66
Category
Article
ISSN
0030-770X

No coin nor oath required. For personal study only.


πŸ“œ SIMILAR VOLUMES


The effect of surface treatments on the
✍ Matteo Dalmiglio; Petra Schaaff; Uwe Holzwarth; Roberto Chiesa; Gianni Rondelli πŸ“‚ Article πŸ“… 2008 πŸ› John Wiley and Sons 🌐 English βš– 174 KB πŸ‘ 2 views

## Abstract Stem modularity in total hip replacement introduces an additional taper joint between Ti‐6Al‐4V stem components with the potential for fretting corrosion processes. One possible way to reduce the susceptibility of the Ti‐6Al‐4V/Ti‐6Al‐4V interface to fretting is the surface modification

The high-cycle fatigue behavior of Ti-6A
✍ R.K. Steele; A.J. McEvily πŸ“‚ Article πŸ“… 1976 πŸ› Elsevier Science 🌐 English βš– 708 KB

Ahatraet-The cyclic stress-strain behavior and the SIN behavior of a "pseudo-elastic" alloy, Ti-6AL-4V of coarsened micros~uct~ and of a "plastic" material, copper, are compared. In accord with views recently put forth by Freudenthal, important differences are noted between these two types of materi