The effect of coupling agent and chemical treatment on rice husk ash- filled natural rubber composites
β Scribed by H. M. Da Costa; L. L. Y. Visconte; R. C. R. Nunes; C. R. G. Furtado
- Publisher
- John Wiley and Sons
- Year
- 2000
- Tongue
- English
- Weight
- 458 KB
- Volume
- 76
- Category
- Article
- ISSN
- 0021-8995
No coin nor oath required. For personal study only.
β¦ Synopsis
Rice husk ash was incorporated into natural rubber (NR) using a laboratory size two-roll mill. Curing using a conventional vulcanization system (CV) was chosen, and cure studies were carried out on a Monsanto rheometer. Physical testing of the NR vulcanizates involved the determination of tensile, tear, and abrasion resistances, and hardness. Fourier transform infrared spectroscopy (FTIR) analysis was done to verify the presence of the characteristic functional groups of precipitated silica in MHA (milled husk ash) and THA (treated husk ash). The effect of the coupling agent, bis(3-triethoxysilylpropyl)-tetrasulfane (Si-69), on the curing and physical properties of the vulcanizates was investigated. A chemical treatment on a rice husk ash was done, and the effects of this procedure are also reported. For comparison, two commercial fillers, precipitated silica (Zeosil-175) and carbon black (N774), were also used. Although the presence of the silane coupling agent had not brought the expected increase in properties, treated husk ash showed exceptional performance in terms of tensile strength and abrasion resistance of the filled vulcanizates.
π SIMILAR VOLUMES
## Abstract Clays belong to an economic class of fillers, which are used extensively in rubbers and plastics. Being nonreinforcing in nature, there are limitations upon its use. If the properties of filler are modified, it will get a higher value as a filler. To achieve this modification of surface
On the basis of results of measurements of physical properties and solvent swelling of the extrudates, it has been observed that epoxidized natural rubber (ENR) interacts chemically with intermediate super abrasion furnace (ISAF) carbon black when the mix of the two was extruded at 130 -160Β°C in a M