𝔖 Bobbio Scriptorium
✦   LIBER   ✦

The effect of copper content and heat treatment on the stress corrosion characteristics of Ai-6Zn-2Mg-X Cu alloys

✍ Scribed by Sarkar, B. ;Marek, M. ;Starke, E. A.


Book ID
112808570
Publisher
The Minerals, Metals & Materials Society
Year
1981
Tongue
English
Weight
972 KB
Volume
12
Category
Article
ISSN
1543-1916