๐”– Bobbio Scriptorium
โœฆ   LIBER   โœฆ

The differential scanning calorimetric study on potentential mid-temperature curing reagent system for epoxy resins

โœ Scribed by Cui Guo-Liang; Wang Wen-Ju


Publisher
Elsevier Science
Year
1988
Tongue
English
Weight
319 KB
Volume
134
Category
Article
ISSN
0040-6031