𝔖 Bobbio Scriptorium
✦   LIBER   ✦

The antioxidation coating of diamond and the strengthening of ceramic grinding tools with a glass-ceramic layer as part of the bonding material

✍ Scribed by Andrzej Szymański; Andrzej Bakon


Publisher
Elsevier Science
Year
1979
Weight
774 KB
Volume
41
Category
Article
ISSN
0025-5416

No coin nor oath required. For personal study only.


📜 SIMILAR VOLUMES


Bonding strength of the apatite layer fo
✍ Juhasz, J. A. ;Best, S. M. ;Kawashita, M. ;Miyata, N. ;Kokubo, T. ;Nakamura, T. 📂 Article 📅 2003 🏛 John Wiley and Sons 🌐 English ⚖ 325 KB 👁 1 views

## Abstract Bioactive glass‐ceramic apatite‐wollastonite (A‐W) has been incorporated into polyethylene in particulate form to create new bioactive composites for potential maxillofacial applications. The effects of varying the volume fraction of glass‐ceramic A‐W filler and the glass‐ceramic A‐W pa