𝔖 Bobbio Scriptorium
✦   LIBER   ✦

Tensile Properties of Ni-Based Superalloy 720Li: Temperature and Strain Rate Effects

✍ Scribed by K. Gopinath; A.K. Gogia; S.V. Kamat; R. Balamuralikrishnan; U. Ramamurty


Publisher
The Minerals, Metals & Materials Society
Year
2008
Tongue
English
Weight
894 KB
Volume
39
Category
Article
ISSN
1073-5623

No coin nor oath required. For personal study only.


πŸ“œ SIMILAR VOLUMES


Effects of strain rate and temperature u
✍ K. F. Wissbrun πŸ“‚ Article πŸ“… 1983 πŸ› Society for Plastic Engineers 🌐 English βš– 486 KB

## Abstract The strength and elongation to break of an acetal copolymer were measured at four elongation rates, from 0.2 to 20 in./min, at temperatures from 239 K to 339 K. Both strength and elongation results could be reduced to master curves by means of time‐temperature superposition. The tempera