Tensile drawing of poly(ethylene-terephthalate)
โ Scribed by J. P. Cavrot; J. C. Engelaere; F. Rietsch
- Publisher
- Springer
- Year
- 1982
- Tongue
- English
- Weight
- 239 KB
- Volume
- 8
- Category
- Article
- ISSN
- 0170-0839
No coin nor oath required. For personal study only.
๐ SIMILAR VOLUMES
Poly(ethylene terephthalate) (PET) fibers with wide range of molecular orientation and crystallinity were prepared by the cold drawing of melt-spun yarns in a temperature-controlled water bath and the subsequent annealing for these samples. For all samples, the true stress-strain curves can be princ
## Abstract The drawing characteristics of poly(ethylene terephthalate) (PET) yarns spun at 1000 and 3000 m/min and film cast at 10 m/min have been studied as functions of drawing temperature up to 200ยฐC and drawing rate up to 50 min^โ1^. The fiber spun at 1000 m/min and the film had very low degre