𝔖 Bobbio Scriptorium
✦   LIBER   ✦

T.C.P. phase particles embedded in a superalloy matrix: Interpretation and prediction of the orientation relationships

✍ Scribed by Pessah-Simonetti, M.; Donnadieu, P.; Caron, P.


Book ID
123047685
Publisher
Elsevier Science
Year
1994
Weight
493 KB
Volume
30
Category
Article
ISSN
0956-716X

No coin nor oath required. For personal study only.