## Abstract Ternary MAX phase Ti~2~SnC was synthesized by Sn‐melt infiltration into a porous preform of sub‐stoichiometric titanium carbide TiC~0.5~. Compared to synthesis starting from elemental Ti + C + Sn mixtures which require temperatures exceeding 1100 °C a significantly lower reaction temper
Synthesis of Ti2SnC at low-temperature using mechanically activated sintering process
✍ Scribed by Shi-Bo Li; Guo-Ping Bei; Hong-Xiang Zhai; Yang Zhou; Cui-Wei Li
- Publisher
- Elsevier Science
- Year
- 2007
- Tongue
- English
- Weight
- 897 KB
- Volume
- 457
- Category
- Article
- ISSN
- 0921-5093
No coin nor oath required. For personal study only.
📜 SIMILAR VOLUMES
A novel biomaterial based on Ti-Si-Zr was developed using the sintering process with a composition targeting at a bulk modulus in the same range as that of human bone, i.e. 10-30 GPa. Control of porosity should also be possible to allow for the promotion osseointegration. The sintering procedure inv
## Abstract One‐dimensional (1D) barium titanate (BaTiO~3~) nanowires, which were uniformly covered with 0D BaTiO~3~ nanocrystals, were synthesized by using a simple solvothermal reaction of protonated trititanate (H~2~Ti~3~O~7~) nanowires with barium hydroxide octahydrate [Ba(OH)~2~·8H~2~O] at 80