Thermostable naphthalate-containing copoly(amide-imide)s with inherent viscosity of 0.53-0.96 dL/g were synthesized by reacting diacid-terminated naphthalate monomers with various diisocyanate-terminated polyimide prepolymers. The polyimide prepolymers were prepared by using 4,4-diphenylmethane diis
Synthesis of thermostable nomex copoly(amide–imide) and their properties
✍ Scribed by Huei-Hsiung Wang; Chen-Chong Su
- Publisher
- John Wiley and Sons
- Year
- 1996
- Tongue
- English
- Weight
- 609 KB
- Volume
- 61
- Category
- Article
- ISSN
- 0021-8995
No coin nor oath required. For personal study only.
📜 SIMILAR VOLUMES
Two series of amorphous fluoro-poly(ether-imide) (6F-PEI) and one series of fluoro-coploy(ether-imide) (6F-CoPEI) polymers based on 2,2bis(3,4-dicarboxyphenyl) hexafluropropane dianhydride (6FDA) and di-ether-containing diamines: 1,2 -bis(4-aminophenoxy)benzene (o-BAPOB) and 4,4 -bis(4-aminophenoxy)
Thermostable polyamideimides with inherent viscosity of 1.02-1.50 dL/g were synthesized from reacting of diamine-terminated aromatic amide prepolymer with various diisocyanate terminated imide prepolymers. The imide prepolymer was prepared by using 4,4'-diphenylmethane diisocyanate to react with 3,3