Synthesis, characterization and molecular weight studies of certain soluble poly(3-alkylthiophene) conducting polymers
β Scribed by Serhan Oztemiz; Gregory Beaucage; Ozcan Ceylan; Harry B. Mark
- Publisher
- Springer
- Year
- 2004
- Tongue
- English
- Weight
- 283 KB
- Volume
- 8
- Category
- Article
- ISSN
- 1432-8488
No coin nor oath required. For personal study only.
π SIMILAR VOLUMES
## Abstract Novel high molecular weight diacetylene (DA) β containing polymers, poly{[bis(3βbutynyl) 3,5βdiynylene sebacate]β__co__β[bis(3βbutynyl) hexamethylenedicarbamate]}s, were synthesized and characterized. The copolymers were found to be semicrystalline and their degree of crystallinity went
## Abstract High molecular weight polyoxyethylene (PEO) was synthesized by using a quaternary catalyst composed of triisobutyl aluminum, phosphoric acid, water, and __N__,__N__βdimethylaniline (DMA). Optimum synthesis conditions and some properties of the product were studied. This catalyst showed