## Abstract The UV‐curable urethane‐acrylates based on 2‐hydroxyethyl methacrylate (HEMA)‐terminated polyurethane (PU) for lithographic and coating applications are investigated in this study. Series of PU prepolymers were made from 4,4‐diphenyl methane diisocyanate (MDI), poly(propylene oxide) gly
Synthesis and properties of UV-curable poly(imideurethane) acrylates
✍ Scribed by M. Meledyn; R. Paszkiewicz; B. Masiulanis
- Publisher
- John Wiley and Sons
- Year
- 2003
- Tongue
- English
- Weight
- 177 KB
- Volume
- 91
- Category
- Article
- ISSN
- 0021-8995
No coin nor oath required. For personal study only.
📜 SIMILAR VOLUMES
## Abstract An dendritic acrylate oligomer with eight double bonds (DAO) was synthesized by Michael addition reaction of ethylene diamine (EDA) and trimethylolpropane triacrylate (TMPTA) under mild conditions, and was easily separated from the reaction system with methanol. The structure of DAO was
Ultraviolet (UV)-curable polyurethane acrylate ionomer (PUAI) prepolymers were synthesized from isophorone diisocyanate (IPDI), poly(methylene ether) glycol (PTMG), 2,2-bis(hydroxymethyl) propionic acid (DMPA), triethylamine (TEA), 2-hydroxy ethyl acrylate (HEA), and dibutyl tin dilaurate (DBT) as a
## Abstract Ultraviolet (UV)/moisture dual‐curable polysiloxane acrylates (PSAs) were prepared from __N,N__‐bis[3‐(triethoxysilyl)propyl]amine (G402) and ethoxylated trimethylolpropane triacrylate (EB160) through Michael addition. The obtained prepolymers were characterized by ^1^H‐NMR and FTIR. Th
A new kind of ultraviolet (UV)-curable waterborne polyurethane-acrylate (PUA) ionomer, prepared from toluene diisocyanate (TDI), polyethylene glycol (PEG), dimethylolpropionic acid (DMPA), triethylamine (TEA), and 2-hydroxyethyl methacrylate (HEMA), was synthesized by the modified prepolymer mixing
Butyl acrylate colloids were obtained by codeposition at 77 K of the monomer with several metals such as Pd, Au, Ag, Cu, Zn, Cd, Ga, In, Ge, Sn, Sb, and Bi. The colloids were polymerized with different amounts of an initiator (AIBN) at 65°C for 0.5 h and a wide range of viscosity-average molecular w