## Abstract Polystyrene‐__graft__‐poly(ethylene glycol) copolymers (PS‐__g__‐PEG) were successfully synthesized using the “grafting‐through” method. The graft copolymers and the surface properties of their coats were characterized by1H‐NMR, gel permeation chromatography (GPC), differential scanning
Synthesis and phase transition of cellulose-graft-poly(ethylene glycol) copolymers
✍ Scribed by Yanxiang Li; Ruigang Liu; Yong Huang
- Publisher
- John Wiley and Sons
- Year
- 2008
- Tongue
- English
- Weight
- 223 KB
- Volume
- 110
- Category
- Article
- ISSN
- 0021-8995
No coin nor oath required. For personal study only.
✦ Synopsis
Abstract
Cellulose‐graft‐poly(ethylene glycol) copolymers were synthesized, and the thermal properties of the copolymers were investigated. The cellulose‐graft‐poly(ethylene glycol) copolymers showed solid–solid phase‐transition behavior with a high thermal storage density and good thermal stability in the temperature region of 25–250°C. The phase‐transition temperature and enthalpy of the cellulose‐graft‐poly(ethylene glycol) copolymers could be adjusted through changes in the poly(ethylene glycol) content. The prepared copolymers could be used as thermal energy storage materials. © 2008 Wiley Periodicals, Inc. J Appl Polym Sci, 2008
📜 SIMILAR VOLUMES
Poly( 1-caprolactone) -poly(ethylene glycol) -poly( 1-caprolactone) triblock copolymers (PECL) covering a wide range of poly(ethylene glycol) (PEG) lengths were synthesized with alkali metal alkoxide derivatives of poly(ethylene glycol). The effects of various factors, such as amount of the initiato
## Abstract Poly(L‐lactide)‐poly(ethylene glycol) multiblock copolymers with predetermined block lengths were synthesized by polycondensation of PLA diols and PEG diacids. The reaction was carried out under mild conditions, using dicyclohexylcarbodiimide as the coupling agent and dimethylaminopyrid
Poly(ethy1ene terephthalate) copolymers were prepared by melt polycondensation of dimethyl terephthalate and excess ethylene glycol with 10- 40 mol% (in feed) of poly(ethy1ene glycol) (E) and poly(tetramethy1ene glycol) (B), with molecular weight (MW) of E and B 200-7500 and 1000, respectively. The