The hydrolytic degradation of two poly(ester amide)s derived from sebacic acid, dodecanediol, and alanine in both the quiral L configuration and the racemic L,D mixture has been studied. The degradation was monitored by following the changes in intrinsic viscosity, mass loss, chemical constitution,
Synthesis and enzymatic degradation of poly(ester-amide) stereocopolymers derived from alanine
✍ Scribed by Minoru Nagata
- Publisher
- John Wiley and Sons
- Year
- 1999
- Tongue
- English
- Weight
- 79 KB
- Volume
- 200
- Category
- Article
- ISSN
- 1022-1352
No coin nor oath required. For personal study only.
📜 SIMILAR VOLUMES
Two poly(ester amides) containing three methoxy groups stereoregularly attached to the main chain have been prepared by using naturally occurring L-arabinose and D-xylose as the starting materials. The polymers were prepared by the active ester polycondensation method and characterized by elemental
A new poly(ester amide) derived from L-alanine has been synthesized and characterized. The polymer has good fiber-and film-forming properties, as well as other characteristics like thermal stability and solubility in chloroform, which enhance its processing facilities. Degradation studies show that
A series of aliphatic poly(ester amide)s derived from 1,6-hexanediol, glycine, and diacids with a variable number of methylenes (from 2 to 8) have been synthesized and characterized. Infrared spectroscopy shows that the studied polymers present a unique kind of hydrogen bond that is established betw
The synthesis and characterization of a series of novel poly(aryl amide imide)s based on diphenyltrimellitic anhydride are described. The poly(aryl amide imide)s, having inherent viscosities of 0.39 -1.43 dL/g in N-methyl-2-pyrrolidinone at 30°C, were prepared by polymerization with aromatic diamine