Synthesis and characterization of model polyether-ester ionomers
β Scribed by Lei Chen; Xue-Hai Yu; Chang-Zheng Yang; Qin Chao Gu; Tian-Dou Hu; Ya-Ning Xie
- Publisher
- John Wiley and Sons
- Year
- 1997
- Tongue
- English
- Weight
- 199 KB
- Volume
- 35
- Category
- Article
- ISSN
- 0887-6266
No coin nor oath required. For personal study only.
β¦ Synopsis
In this study, a series of polyether-ester ionomers was prepared by neutralizing the carboxylic acid groups in 1 : 1 copolymers of benzenetracarboxylic dianhydride (BTDA) and poly(tetramethylene oxide) or poly(ethylene oxide) glycol. The base polymers were in a liquid state while the ionomers were in solid state and a separate ionic phase was formed. The local structure and the morphology of the ionomers were investigated by dynamic mechanical analysis, Fourier transform infrared spectroscopy, and small-angle x-ray scattering as well as extended x-ray absorption fine structure. Clearly, the geometric structure of the ionic sites varied with the nature of the metal ions and the morphology of the ionomers was determined by the microstructure of the ion aggregates.
π SIMILAR VOLUMES
## SYNOPSIS A series of polyether (PTMO, PEO) polyurethane ionomers having different contents of sodium sulfonate groups in the soft segments have been synthesized. The reaction of transesterification was involved in the incorporation of the sodium sulfonate groups in the polyether. The polyuretha
A new kind of ultraviolet (UV)-curable waterborne polyurethane-acrylate (PUA) ionomer, prepared from toluene diisocyanate (TDI), polyethylene glycol (PEG), dimethylolpropionic acid (DMPA), triethylamine (TEA), and 2-hydroxyethyl methacrylate (HEMA), was synthesized by the modified prepolymer mixing
A series of starch and amylose esters with different degrees of substitution and side-chain length were prepared and studied. The esters were prepared by acylation of the polysaccharide with the appropriate acid chlorides, such as octanoic, dodecanoic, and octadecanoic. The degrees of substitution w
The modification of PVC with 4-mercaptopyridine is described. The content of pyridine groups in the products is measured by NMR and IR spectroscopy. The degree of modification depends on the reaction conditions, and values of up to 70% are achieved without degradation or other appreciable side react