𝔖 Bobbio Scriptorium
✦   LIBER   ✦

Susceptibility to pitting corrosion and corrosion cracking of steels alloyed with molybdenum, silicon, and boron

✍ Scribed by S. A. Glazkova; G. L. Shvarts


Publisher
Springer
Year
1971
Tongue
English
Weight
377 KB
Volume
7
Category
Article
ISSN
0009-2355

No coin nor oath required. For personal study only.


πŸ“œ SIMILAR VOLUMES


The effect of sulfide inclusions on the
✍ Prof. Dr. Z. Szklarska-Ε›mialowska; Dr. E. Lunarska πŸ“‚ Article πŸ“… 1981 πŸ› John Wiley and Sons 🌐 German βš– 974 KB

## Abstract Recent opinions on the effect of nonmetallic inclusions, especially sulfides, on the nucleation of pits, stress corrosion cracks, and hydrogen‐induced cracks are reviewed. The nonmetallic inclusions present in steels as impurities adversely affect the corrosion resistance of steels. Th

Pitting, Crevice and stress corrosion re
✍ Dr. M. B. Rockel; Dipl.-Ing. M. Renner πŸ“‚ Article πŸ“… 1984 πŸ› John Wiley and Sons 🌐 German βš– 405 KB πŸ‘ 1 views

## Abstract This paper presents new data on the resistance of recently developed high‐alloy stainless steels to localised corrosion in chloride solutions. Pitting potential was determined in artificial sea water, and critical pitting temperature CPT in very aggressive FeCl~3~ solution. Critical cre