From supported homogeneous catalysts to
β
Agnès Choplin; Françoise Quignard
π
Article
π
1998
π
Elsevier Science
π
English
β 338 KB
Numerous methods are now available for the synthesis of a large variety of heterogeneous molecular catalysts. Their specific domain of application, and the main advantages and drawbacks of these solids are briefly analyzed here.