Surface analysis of poly(vinyl chloride)/poly(α-methylstyrene-co- acrylonitrile) blends by X-ray photoelectron spectroscopy

✍ Scribed by S.H. Goh; H.S.O. Chan; K.L. Tan


Publisher
Elsevier Science
Year
1991
Tongue
English
Weight
197 KB
Volume
52
Category
Article
ISSN
0169-4332