Surface analysis of AgSn alloys by ESCA
✍ Scribed by R. Holm; S. Storp
- Publisher
- Elsevier Science
- Year
- 1976
- Tongue
- English
- Weight
- 595 KB
- Volume
- 8
- Category
- Article
- ISSN
- 0368-2048
No coin nor oath required. For personal study only.
📜 SIMILAR VOLUMES
The surface properties of Ag,Sn are important in the amalgamation process so that mechanical abrasion is generally necessary to get a satisfactory amalgam. Therefore, the present study was undertaken to characterize the surface of Ag3Sn after several types of surfaces treatments. Homogeneous polycr