𝔖 Bobbio Scriptorium
✦   LIBER   ✦

Surface analysis by scanning tunnelling microscopy: A M Baró,Dpto de Fisica Fundamental, C-III, Universidad Autónoma de Madrid, Cantoblanco, 28049-Madrid, Spain


Publisher
Elsevier Science
Year
1987
Tongue
English
Weight
146 KB
Volume
37
Category
Article
ISSN
0042-207X