𝔖 Bobbio Scriptorium
✦   LIBER   ✦

Surface analysis and anti-graffiti behavior of a weathered polyurethane-based coating embedded with hydrophobic nano silica

✍ Scribed by A. Mohammad Rabea; M. Mohseni; S.M. Mirabedini; M. Hashemi Tabatabaei


Book ID
116244972
Publisher
Elsevier Science
Year
2012
Tongue
English
Weight
357 KB
Volume
258
Category
Article
ISSN
0169-4332

No coin nor oath required. For personal study only.