𝔖 Bobbio Scriptorium
✦   LIBER   ✦

Supplement on “Effects of heat-flux features on the differential scanning calorimetry curve of a thermoelastic martensitic transformation”

✍ Scribed by Márton Benke; Valéria Mertinger; Ferenc Tranta; Péter Barkóczy; Lajos Daróczi


Publisher
Elsevier Science
Year
2010
Tongue
English
Weight
291 KB
Volume
527
Category
Article
ISSN
0921-5093

No coin nor oath required. For personal study only.


📜 SIMILAR VOLUMES