Superalloys 2012 (Huron/Superalloys) || Weld Solidification Behavior of Ni-Base Superalloys for use in Advanced Supercritical Coal-Fired Power Plants
✍ Scribed by Huron, Eric S.; Reed, Roger C.; Hardy, Mark C.; Mills, Michael J.; Montero, Rick E.; Portella, Pedro D.; Telesman, Jack
- Book ID
- 120480956
- Publisher
- John Wiley & Sons, Inc.
- Year
- 2012
- Tongue
- English
- Weight
- 966 KB
- Edition
- 1
- Category
- Article
- ISBN
- 0470943203
No coin nor oath required. For personal study only.
✦ Synopsis
A Superalloy, Or High-performance Alloy, Is An Alloy That Exhibits Excellent Mechanical Strength At High Temperatures. Superalloy Development Has Been Driven Primarily By The Aerospace And Power Industries. This Compilation Of Papers From The Twelfth International Symposium On Superalloys, Held From September 9-13, 2012, Offers The Most Recent Technical Information On This Class Of Materials.