𝔖 Bobbio Scriptorium
✦   LIBER   ✦

Subsurface deformation during Vickers indentation of bulk metallic glasses

✍ Scribed by S. Jana; U. Ramamurty; K. Chattopadhyay; Y. Kawamura


Publisher
Elsevier Science
Year
2004
Tongue
English
Weight
224 KB
Volume
375-377
Category
Article
ISSN
0921-5093

No coin nor oath required. For personal study only.


πŸ“œ SIMILAR VOLUMES


Stick–slip behavior of serrated flow dur
✍ Florian H. Dalla Torre; David KlaumΓΌnzer; Robert Maaß; JΓΆrg F. LΓΆffler πŸ“‚ Article πŸ“… 2010 πŸ› Elsevier Science 🌐 English βš– 910 KB

Accurate compression tests with a piezoelectric load cell and an acquisition rate of up to 10 kHz were performed on a Zr-based bulk metallic glass in the temperature range 210-320 K at a strain rate of 10 Γ€3 s Γ€1 . Information about the stress drop magnitude and the associated size of shear displace